Trial Mix Batch Book — Lab Batch Weights

Convert your 1 cubic metre mix design into laboratory trial batch weights: 50 L batch of cement 320 / fly ash 80 / sand 780 / aggregates 1270 / water 160

Trial Mix Batch Book

Turn your 1 m³ mix design into a weigh-batcher-ready trial batch sheet. SSD-to-wet aggregate conversion, free-water credit and admixture dose in mL. Pure arithmetic; your mix stays yours.

Trial mix batch — tilting-drum mixer on a stand with ingredients falling in and a rotation arrow

Mix design per m³ (SSD basis, kg)

Aggregate moisture (%)

Water absorption, SSD (%) , from your aggregate test report

Free moisture = moisture − absorption. Wet stock (moisture > absorption) carries surface water: credited against batch water. Dry stock (moisture < absorption) absorbs the deficit from the mix. Added back so your water–binder ratio holds.

Batch sheet: L (factor )

Cement
kg
Fly ash
kg
GGBS
kg
Sand (SSD / wet)
/ kg
20 mm (SSD / wet)
/ kg
10 mm (SSD / wet)
/ kg
Water (design / to batch)
/ L
Free water carried (deducted)
L
Absorption deficit (added back)
L
Admixture
mL

How this is calculated

Every ingredient is multiplied by the batch factor (batch litres ÷ 1000). Moisture correction follows standard lab practice: weigh aggregates at their moist stock mass, SSD × (1 + moisture%), and credit the free water they carry against the batch water, so the water–binder ratio you designed is the one you actually batch.

Admixture is dosed as % of total binder (cement + fly ash + GGBS) and read in mL (≈1 kg/L). This tool does arithmetic only — the mix design itself must come from your IS 10262 spreadsheet or consultant.

Worked example

Given: M25-ish trial: cement 320, fly ash 80, sand 780, 20 mm 860, 10 mm 410 kg/m³, water 160 L, PCE at 1.2% of binder; batch 50 L; sand at 3% moisture with 1.2% SSD absorption: 1.8% free.

Factor 0.05 → cement 16.0 kg, fly ash 4.0 kg, sand 39.0 SSD → 40.17 kg wet

Free water from sand = 1.17 L → batch water = 8.0 − 1.17 = 6.83 L

Admixture = 400 × 1.2% × 0.05 = 0.24 kg = 240 mL

FAQ

What batch volume should a lab trial use?

30–60 L is typical: enough for three 150 mm cubes plus slump and density tests, small enough to mix by hand or pan mixer. Keep the batch at least 25 L so weighing errors on the smallest ingredient (admixture) stay proportionate.

Why does wet sand weigh more but water go down?

Wet sand carries water on its surface. If you batch the SSD weight from moist stock you would short the aggregate and add the design water on top: raising the effective w/c. Weighing wet and deducting the carried moisture keeps both the aggregate content and the w/c exactly as designed.

My moisture value is above 12% — now what?

That is likely a wet-washed or rain-soaked stock with running water in the pores, not surface moisture: the simple correction no longer holds. Drain the stockpile, re-test moisture, and batch the next day. The tool caps at 12% for exactly this reason.

Should trials use the same admixture as production?

Yes: same product, same dose basis. Changing the admixture between trial and production invalidates the workability and strength relationship the trial exists to establish. Record brand, type and dose on every batch sheet.

§ 99

Calculator companions

Often used together with this calculator. Pick the next step in your design or QA loop.

Visualisation

Updates live from the calculator above. Click Make batch sheet to refresh.

This is the same calculator ConcreteInfo publishes on the main site. It runs in your browser, with no account and nothing to install.